Cooling Tower Restoration — Dallas, Texas
A relatively new cooling tower at a major Dallas hotel suffered severe premature corrosion after exposure to an aggressive chemical environment. In several areas, the original sheet metal had deteriorated enough to require reinforcement before the tower could be fully restored and protected.
The Challenge
The tower showed extensive corrosion despite being relatively new equipment. Chemical attack had weakened portions of the metal and created the risk of continued deterioration, leaks, and eventual equipment replacement if the damage was not stopped.


The Dynesic Solution
The damaged areas were mechanically prepared to remove loose corrosion and create a sound surface profile. Severely weakened sections were reinforced with new sheet metal, then the restored surfaces were protected with a Dynesic coating system selected for long-term chemical and corrosion resistance.
The Result
The cooling tower was restored without the cost and disruption of premature replacement. Structurally weakened areas were rebuilt, active corrosion was stopped, and the completed Dynesic system provided a durable barrier against continued chemical attack.
The result: a cooling tower stronger, better protected, and ready to return to service.
Better Protected Than New.
Equipment saved. Corrosion stopped. Chemical protection upgraded.